Select Page

info@solventrs.com

(847) 833-7010

Most corrosion protection packaging specifications are a product name and a size. Somebody rusted a shipment once, a supplier recommended a bag, and the bag went into the packing instruction. It works until the part changes, or the storage time doubles, or a customer audit asks why that bag and not another one, and nobody in the building can answer.

Cortec® Case History #878 describes a buyer who went about it the other way around, and the sequence is worth copying whether or not your parts look anything like theirs.

What the case describes

A manufacturer of radioactive waste containers needed to preserve roughly 12 tonnes of steel for two years. The application fell under French PMUC requirements for materials used in nuclear installations, which meant the preservation system itself had to clear an approval process before it could be used at all. Two constraints came out of that: the materials had to be sulfur-free and halogen-free.

The system adopted had three parts, addressing the inside and the outside of each container separately:

  • The container was washed with VpCI®-415, a biodegradable heavy-duty alkaline degreaser.
  • BioPad® was placed inside the container to provide vapor phase corrosion inhibition in the enclosed volume.
  • A Cortec VpCI® film was applied to the exterior.

The buyer ran this as a six-month pilot first. Only after the pilot did the preservation system get adopted across 40 cylinders.

Three things that specification got right

It started with the wash, not the wrap

The cleaning step is first in the sequence and it is not incidental. Vapor phase inhibitors adsorb onto metal; they do not displace a film of cutting fluid, drawing compound, fingerprint salts or weld smut to get there. A contaminated surface under a good bag is still a contaminated surface, and the residue underneath often carries the chlorides that start the pit. This is the single most common reason a packaging change fails to fix a rust problem: the packaging was never the problem.

It is also the step most likely to be missing from an inherited spec, because cleaning usually belongs to a different department than packaging.

It treated inside and outside as separate problems

A large fabricated vessel has an enclosed interior volume and an exposed exterior, and those two surfaces fail for different reasons on different timelines. The interior is a closed box where a vapor phase emitter is efficient and nothing else is practical, because no sprayed coating reaches every internal surface and no one is going to open a sealed container for inspection. The exterior is handled, strapped, rained on and abraded, so it needs a physical barrier film.

Specifying one product for both is how a spec ends up over-protecting one surface and under-protecting the other.

It wrote the material restrictions into the requirement

Sulfur-free and halogen-free were not preferences; they were pass or fail criteria from the industry the parts were going into. Writing restrictions that way, up front, is what makes a specification defensible later. The same logic applies well outside nuclear work: food and beverage equipment, medical device components, electronics assemblies and anything going into a painted or plated downstream process all carry restrictions on what may be left on the surface, and those restrictions belong in the packaging spec rather than in somebody’s memory.

Running the same pilot in your plant

  1. Write down the duration and the environment. Two years in a covered yard is a different specification from six months in a heated warehouse. Most rust failures trace back to a spec written for the second and used for the first.
  2. List your restrictions before you look at products. What may not be left on the surface, what the downstream process is, what the receiving customer has to do to the part before using it.
  3. Fix the cleaning step. Decide what the part is washed in, at what concentration, and how it is dried before packaging. If you are checking cleaner strength by eye, our concentration testing guide has the refractometer procedure and the target ranges.
  4. Separate interior and exterior. Size the interior emitter to the enclosed cubic footage. Choose the exterior film for handling and weather, not for what is already on the shelf.
  5. Pilot on a real unit for a real duration. Six months on one container told the buyer in Case History #878 more than any salt spray number would have. Open it, photograph it, and keep the photographs.
  6. Then write the spec and roll it out. Part number, cleaner and concentration, emitter type and count, film type and gauge, seal method, and the restrictions that drove each choice.

Which products

If you need help matching a product to a metal and an exposure, the VpCI product selection guide lays it out by metal type and environment severity.

On the cleaning step: if the wash in your current process is a parts tank somebody tops up by feel, that is the part of the specification to fix first. Our line of Build-All and Magido aqueous parts washers runs the Cortec alkaline cleaners at a controlled concentration and temperature, which is what makes the cleaning step repeatable enough to write into a specification at all.

We can help you draft the packaging instruction, size the emitters, and put together a pilot quantity so you have photographs instead of assumptions six months from now. Contact Solvent Recycling Systems.

Source: Cortec Case History #878, as summarized publicly by Cortec. The customer is not named by Cortec and is not named here.