There is a specific kind of inventory that nobody plans for and everybody eventually has. It is not raw stock and it is not finished goods. It is good parts that have nowhere to go, because something downstream of them stopped.
Cortec® described one version of this in Case History #874. A major automaker hit a raw material shortage that forced vehicle assembly to a halt. Rather than idle everything, the company kept manufacturing the components that were not affected by the shortage, including axles and engines, and held them. Cortec’s published account is that VpCI® packaging preserved those parts for six to twelve months while the company waited for supply conditions to recover.
That decision is worth looking at closely, because the reasoning is not really about corrosion. It is about keeping a plant running when the bottleneck is somewhere you do not control.
The real problem is that the storage was not planned
Parts that were built to move within a week get packaged to move within a week. That usually means a cardboard box, a bag that is there to keep chips out, and whatever residual coolant or wash-line film happens to be on the part when it leaves the line. None of that is a storage system. It is handling.
Hold those same parts for six months and three things go wrong at once. Humidity cycles inside the packaging as the building heats and cools, so moisture condenses on the coldest metal in the box. Any residual process fluid on the part becomes a corrosion site rather than a protective film, because most coolants and cleaners are not rust preventatives and some are mildly aggressive once they concentrate. And machined surfaces, which are the expensive part of the part, are exactly the surfaces with no mill scale, no paint and no protection at all.
What makes this situation harder than ordinary long-term storage is that you usually do not know the duration when you start. Nobody in that automaker’s plant knew on day one whether this was a six-week hold or a twelve-month hold. That argues for packaging to the longer case, because re-packaging a warehouse of finished components later is a cost nobody budgets and a handling risk on top.
What a six-to-twelve-month hold actually needs
The approach Cortec documents in cases like this is consistent, and it is not complicated. There are four decisions.
- Get the process fluid off first. This is the step that gets skipped and the step that causes most failures. Vapor phase inhibitor needs to reach bare metal. Coolant, drawing compound or shop soil sitting between the metal and the inhibitor is a barrier, and in some cases it is itself the corrodent. A clean, dry part is the precondition for everything below.
- Pick a barrier that carries the inhibitor. VpCI film or VpCI paper does two jobs — it is the physical enclosure and it is the source of the vapor phase inhibitor that adsorbs onto every surface inside, including the surfaces the packaging never touches. A plain poly bag does only the first job.
- Close the enclosure. Vapor phase protection is only as good as the container. A zip-close bag that is actually closed outperforms a much better film left open. This is also why pallet loads and returnable containers usually need an emitter or a liner rather than relying on individual bags that get opened for counts.
- Manage humidity where the swing is severe. In an unconditioned warehouse through a Midwest winter and spring, pairing a desiccant with the vapor inhibitor removes the condensation driver rather than only inhibiting its effect.
The one thing we would add from our own customers’ experience: label the packages with the date they were packed and what is inside. A twelve-month hold outlives the memory of whoever packed it, and parts that get opened for an inspection and then re-closed badly are a common source of the rust that shows up at the end.
Which products do this
These are the items most of our customers use for a multi-month hold on machined components. Sizes shown are the common ones; the full ladder of widths, gauges and formats is on each listing.
- Cortec® VpCI®-126 blue zip-close bag, 12″ x 12″, 4 mil — the default for individually bagged parts, and the easiest thing to standardize on
- Cortec® VpCI®-146 multimetal VCI kraft paper, 35#, 36″ x 1,200′ — for interleaving, wrapping and lining crates and returnable containers
- Cortec® VpCI®-105 emitter cup, 5 cu ft — for enclosures and containers you cannot bag, including control cabinets shipped with the assembly
- Cortec® Cor-Pak® breathable VpCI pouch, 8 ft³ — a simple way to carry inhibitor into a box without changing the box
- Cortec® Desicorr® VpCI® pouch, 1/6 unit — desiccant and vapor inhibitor in one pouch, for unconditioned storage
- Cortec® VpCI®-377 water-based rust preventative concentrate, 5 gallon — where the part needs a film on it before it goes in the bag
- VpCI product selection guide — to match the metal and the storage environment before you commit to a format
The cleaning step is the one we get called about
Almost every rust complaint we investigate on VCI-packaged parts comes back to what was on the part when it was packaged, not to the packaging. That is the least glamorous finding in this business and it is consistently true.
If a shortage or a shutdown has just turned your line into a parts warehouse, the practical question is whether you have the capacity to clean and dry parts at the rate you are producing them, in the window before they go into storage. A plant that was washing parts just well enough for immediate assembly is usually not set up for that. Our Build-All and Magido aqueous parts washers are built in Milwaukee and sized for exactly this kind of batch work, and we would rather talk about it before the parts are on the shelf than after.
For the packaging sequence itself, our walkthrough on how to prep and pack metal parts for rust-free shipment covers the handling order, and sizing Desicorr VpCI pouches covers the humidity side.
If you are holding inventory you did not plan to hold
Tell us what the parts are, what they are made of, how they are packaged today and roughly how long you expect to sit on them. We will tell you what changes and what does not, and in a lot of cases the answer is a different bag rather than a new process. Contact Solvent Recycling Systems and we will size it with you.